(PresseBox) - Plastic is increasingly being used as a construction material and must therefore be able to withstand ever greater loads. Apart from static and dynamic tests, the performing of creep tests on plastics is therefore gaining in importance in research. In order to implement a wide range of tests on plastics, the Department for Polymer Materials at the University of Bayreuth uses a testing machine from the company Messphysik - a member of the Zwick Roell Group.
Determining creep behavior has become essential for the development of new materials in the plastics sector. In the testing machine of the University of Bayreuth, up to six specimens can be loaded simultaneously in tensile, compression and 3-point flexure. This allows the change in the material's properties over time to be determined at constant elongation (relaxation) and at constant tension (retardation) as well as under the influence of temperature. Apart from these pure creep test loads, various load profiles can also be applied. At the Department for Polymer Materials, a wide range of materials are tested, such as elastomers, composite materials and thermoplastics.
In order to be able to make a statistically covered statement as quickly as possible, up to six specimens are tested in this testing machine simultaneously. As a standardized test typically last 33 days (1000 hours), this is a decisive advantage. To further shorten the test duration, an attempt is also made to extrapolate the test results to 1000 hours after a shorter time.
The deformation of the specimens is measured contactlessly with a video extensometer, both at room temperature and at an elevated temperature. For this, the testing machine is equipped with a temperature chamber, which enables tests between -50°C and +250°C. With the test software testXpert® II in combination with the measuring, control and regulating electronics testControl, all required test procedures and evaluations can be freely defined.






Themen in dieser Pressemitteilung:


Unternehmensinformation / Kurzprofil:



Leseranfragen:



PresseKontakt / Agentur:



drucken  als PDF  an Freund senden  HA67 6:1 Heat Shrinkable Tubing - The best choice for large diameter differences
Capacity and quality up, costs down
Bereitgestellt von Benutzer: PresseBox
Datum: 17.05.2011 - 09:39 Uhr
Sprache: Deutsch
News-ID 1023579
Anzahl Zeichen: 0

contact information:
Contact person:
Town:

Ulm


Phone:

Kategorie:

Family


Anmerkungen:


Diese Pressemitteilung wurde bisher 316 mal aufgerufen.


Die Pressemitteilung mit dem Titel:
"Creep test: Plastics under continuous loading
"
steht unter der journalistisch-redaktionellen Verantwortung von

Zwick GmbH&Co. KG (Nachricht senden)

Beachten Sie bitte die weiteren Informationen zum Haftungsauschluß (gemäß TMG - TeleMedianGesetz) und dem Datenschutz (gemäß der DSGVO).


Alle Meldungen von Zwick GmbH&Co. KG



 

Who is online

All members: 10 721
Register today: 0
Register yesterday: 0
Members online: 0
Guests online: 199


Don't have an account yet? You can create one. As registered user you have some advantages like theme manager, comments configuration and post comments with your name.